新疆呼图壁储气库埋地管道防腐对策研究
分享到:

《石油管材与仪器》[ISSN:2096-0077/CN:61-1500/TE]

卷:
5
期数:
2019年02期
页码:
59-61
栏目:
储气库专题
出版日期:
2019-04-20

文章信息/Info

Title:
Application Analysis of Anticorrosion of Buried Pipeline in Xinjiang Hutubi Gas Storage
文章编号:
2096-0077(2019)02--0059-03
作者:
张哲王明锋林敏张海明陈月娥刘进博
中国石油新疆油田公司 新疆 克拉玛依 834000
Author(s):
ZHANG Zhe WANG Mingfeng LIN Min ZHANG Haiming CHEN Yue′e LIU Jinbo
PetroChina Xinjiang Oilfield Company,Karamay,Xinjiang 834000,China
关键词:
埋地管线游离水CO2分压内防腐外防腐阴极保护
Keywords:
buried pipelinefree waterCO2 partial pressureinternal corrosion protectionexternal corrosion protectioncathodic protection
分类号:
TE372
DOI:
10.19459/j.cnki.61-1500/te.2019.02.014
文献标志码:
A
摘要:
新疆呼图壁储气库埋地管线输送介质以甲烷为主,其中CO2占1.89%,采气工况下伴有凝析油和地层水产出,埋地管道易受腐蚀影响。为掌握其腐蚀状况以采取合理防腐措施,通过对腐蚀环境分析研究,确定其腐蚀影响因素以游离水、CO2分压为主,还包括土壤环境、温度、氯离子浓度和流速等。对此,储气库采取“不锈钢双金属复合管+3PE防腐层+强制电流”的防腐措施,每年检修期间对埋地金属管线进行检测,对个别破损点及时修复维护,保证气库安全平稳运行。
Abstract:
The Xinjiang Hutubi gas storage is a depletion type of oil&gas reservoirs.The total length of buried injectionproduction pipelines and injectionproduction main lines is 39.4km,the medium is mainly methane,with carbon dioxide accounting for 1.89%.During the period of gas extraction,there will be accompanied by the production of condensate oil and formation water.Under the influence of the partial pressure of carbon dioxide and formation water,the buried metal pipelines is vulnerable to corrosion.For the study of corrosion status of buried pipeline and adopt reasonable anticorrosion measures,through the analysis of corrosive environment,the gas storage corrosion factors are priority to with free water,CO2 partial pressure,also including the soil environment,temperature,concentration of chloride ion and flow rate etc.In this regard,gas storage take”internal corrosion protection+external corrosion protection+cathodic protection”combination of anticorrosion,that is “stainless steel double metal composite pipe+3PE anticorrosion layer+forced current”approach.During the overhaul period,the buried metal pipeline is detected,repair and maintain the individual damaged spots in time,ensure the safe and smooth operation of the gas storage.

参考文献/References:

[1]丁国生,李春,王皆明,等.中国地下储气库现状及技术发展方向[J].天然气工业,2015,35(11):107-112.
[2] 杨琴,徐清秀,银小兵,等.枯竭气藏型地下储气库工程安全风险与预防控制措施探讨[J].石油与天然气化工,2011,40(4):410-412.
[3] 冯鹏,王俊,侯晓犇.储气库用注采管汇腐蚀因素分析[J].腐蚀研究,2013,27(4):47-50.
[4] 林存瑛.天然气矿场集输[M].北京:石油工业出版社,1997.
[5] 卜明哲,陈龙,刘欢,等.高含CO2储气库集输管道腐蚀防护研究[J].当代化工,2014,43(2):230-231.
[6] 高文玲.管道腐蚀检测及强度评价研究[D].西安:西安石油大学,2011.
[7] 张卫兵,刘欣,王新华,等.苏桥储气库群高压、高温介质管道腐蚀控制措施[J].科技资讯,2012,(2):120-122.
[8] 李林辉,李浩,屠海波,等.油气集输管线内防腐技术[J].上海涂料,2011,49(5):31-33.
[9] 薛致远,毕武喜,陈振华,等.油气管道阴极保护技术现状与展望[J].油气储运,2014,33(9):938-944.
[10] 刘志军,杜全伟,王维斌,等.埋地保温管道阴极保护有效性影响因素及技术现状[J].油气储运,2015,34(6):576-579.

备注/Memo

备注/Memo:
第一作者简介:张哲,男,1984年生,2008年毕业于大庆石油学院,工学学士,工程师,目前主要从事天然气地面工艺处理方向工作。 E-mail:zzhe3@petrochina.com.cn
更新日期/Last Update: 2019-04-25